wiki:troubleshooting_bed-adhesion-tips [2026/01/21 00:45] – created page samurailink3wiki:troubleshooting_bed-adhesion-tips [2026/01/26 19:28] (current) – [Other Tips and Tricks] dc
Line 17: Line 17:
 Dehydrating a roll of filament can sometimes be enough to bring it back to life. Dehydrating a roll of filament can sometimes be enough to bring it back to life.
  
 +==== Other Tips and Tricks ====
 +Some tips from other Whistle Crew volunteers:
  
 +  * Increasing wall count to "3"
 +  * For PLA, set/reduce initial lay print speeds to 30mm/s and 70mm/s for the first layer infill
 +  * Increasing the first layer bed temp 5c to 10c, for example increase to 60-65c (from 55c) for PLA on a textured PEI plate
 +  * For Silk PLA, set Initial Layer Speed to 20mm/s, bump first layer bed temp to 75c and the rest at 70c
 +  * Use nitrile-coated gloves when handling the build plate to keep it free from finger oils
  
wiki/troubleshooting_bed-adhesion-tips.1768956359.txt.gz · Last modified: by samurailink3

Except where otherwise noted, content on this wiki is licensed under the following license: Public Domain
Public Domain Donate Powered by PHP Valid HTML5 Valid CSS Driven by DokuWiki